Performance, durability, and leachability of high-strength concrete incorporating red mud and ground granulated blast furnace slag

Document Type : Reply to comment on Paper

Authors
1 Research Group of Environmental Engineering and pollution Monitoring, Research Center for Environment and Sustainable Development, Tehran, Iran.
2 Department of Environmental Engineering, College of Environment, Karaj, Iran.
10.22059/ijmge.2026.419744.595415
Abstract
This study investigated the feasibility of using red mud (RM) and ground granulated blast furnace slag (GGBFS) as partial cement replacements in high-strength concrete, with emphasis on workability, compressive strength, durability, microstructural development, and environmental safety. Response surface methodology was applied using a custom 18-run experimental matrix to investigate three mix-design factors: RM replacement at 0, 7.5, and 15%, GGBFS replacement at 0, 10, and 20%, and w/b ratios of 0.30, 0.375, and 0.45. The matrix included three plain-cement control mixtures at the three w/b levels. The resulting responses were evaluated using second-order polynomial models and analysis of variance (ANOVA).The mixtures were evaluated by slump, compressive strength at 7, 28, and 56 days, water absorption, electrical resistivity, chloride migration, XRD, SEM, and TCLP analyses. The results show that GGBFS generally improved workability, while RM reduced slump, particularly in mixtures with lower water-to-binder ratios. Although cement replacement slightly decreased compressive strength, most blended mixtures still reached the performance range expected for high-strength concrete, especially at lower water-to-binder ratios. The blended binders also showed clear later-age strength gain, reflecting continued hydration and pozzolanic activity. Bulk electrical resistivity decreased with increasing RM content; however, by separating pore-solution conductivity from pore geometry through the formation-factor concept, this decrease was shown to originate mainly from the higher alkali (Na⁺, K⁺, OH⁻) concentration of the pore solution rather than from a coarser pore network. Consistently, the chloride migration coefficient decreased, indicating combined pore refinement and enhanced chloride binding in the aluminate-rich binder. XRD and SEM results confirmed modified hydration behavior through reduced visible portlandite and increased formation of matrices rich in C-S-H and C-A-H. TCLP results further showed that heavy-metal concentrations remained below regulatory limits. Overall, the findings support RM and GGBFS as viable components of a more sustainable high-strength concrete binder system when mixture proportions are carefully controlled. Within the tested domain, a mixture with 7.5% RM, 20% GGBFS and a water-to-binder ratio of 0.30 provided the best compromise between mechanical performance, transport resistance and clinker reduction (27.5% cement replacement, 85.3 MPa at 56 days, 373.8 Ω·m, and a chloride migration coefficient of 4.15 × 10⁻¹² m²/s).
Keywords
Subjects

[1]. Global Cement and Concrete Association, Cement and concrete around the world. 2026: [Online]. Available: https://gccassociation.org/concretefuture/cement-concrete-around-the-world/.
[2]. The Concrete Center, Whole-Life Carbon and Buildings, in TCC/05/30. 2016, London, UK: MPA The Concrete Centre.
[3]. Scrivener, K.L., John, V.M., and Gartner, E.M., Eco-efficient cements: Potential economically viable solutions for a low-CO2 cement-based materials industry. Cement and Concrete Research, 2018. 114: p. 2-26.DOI: 10.1016/j.cemconres.2018.03.015.
[4]. Marin, O.A., Kraslawski, A., and Cisternas, L.A., Estimating processing cost for the recovery of valuable elements from mine tailings using dimensional analysis. Minerals Engineering, 2022. 184: p. 107629.DOI: https://doi.org/10.1016/j.mineng.2022.107629.
[5]. Gou, M., et al., Utilization of tailings in cement and concrete: A review. Science and Engineering of Composite Materials, 2019. 26(1): p. 449-464.DOI: https://doi.org/10.1515/secm-2019-0029.
[6]. Gayana, B. and Chandar, K.R.J., Sustainable use of mine waste and tailings with suitable admixture as aggregates in concrete pavements-A review. Advances in concrete construction, 2018. 6(3): p. 221.DOI: 10.12989/acc.2018.6.3.221.
[7]. Shirdam, R., Geotechnical Investigation of Tailings Disposal Site for Tailings Storage of zinc Processing Factory. Pollution, 2022. 8(1).DOI: 10.22059/POLL.2021.320134.1029.
[8]. Shirdam, R. and Nezami, A., Stabilization and Solidification of Produced Tailings in the Lead Extraction Process Using Brine Leaching Method. Environment Interdisciplinary Development, 2024. 9(85): p. 43-63.DOI: https://doi.org/10.22034/envj.2024.458444.1380.
[9]. Pujar, S.M. and Prakash, K., Effect of replacement of cement by red mud on the properties of concrete. International Journal of Scientific Engineering Research, 2014. 5(9): p. 805-816.
[10]. Singh, J., Effect of red mud as cement replacement on the properties of concrete. International Journal of Innovations in Engineering Technology, 2019: p. 2319-1058.DOI: http://dx.doi.org/10.21172/ijiet.151.08
[11]. Ribeiro, D.V., Labrincha, J.A., and Morelli, M.R.J.M.r., Potential use of natural red mud as pozzolan for Portland cement. 2011. 14: p. 60-66.DOI: https://doi.org/10.1590/S1516-14392011005000001.
[12]. Shirdam, R., Sadeghi, B, Rad, M. R., Bakhshi, N., Mirzaei, H. A., Reusing red mud waste and low grade bauxite as raw materials for brick manufacturing by experimental design technique. International Journal of Environment and Waste Management, 2021. 27(1): p. 46-60.DOI: 10.1504/ijewm.2021.111907.
[13]. Saafan, M.A., Etman, Z.A., and El lakany, D.M., Microstructure and Durability of Ground Granulated Blast Furnace Slag Cement Mortars. Iranian Journal of Science and Technology, Transactions of Civil Engineering, 2020. 45(3): p. 1457-1465.DOI: 10.1007/s40996-020-00533-3.
[14]. Sang, N.T. and Khoa, N.T. Experimental study on effect of ground granulated blast furnace slag of strength and durability of sand concrete. in CIGOS 2019, Innovation for Sustainable Infrastructure: Proceedings of the 5th International Conference on Geotechnics, Civil Engineering Works and Structures, Singapore, p. 409-414. DOI: 10.1007/978-981-15-0802-8_63. 2019. Springer.
[15]. Esmaeili, J. and Aslani, H., Use of copper mine tailing in concrete: strength characteristics and durability performance. Journal of Material Cycles and Waste Management, 2019. 21(3): p. 729-741.DOI: 10.1007/s10163-019-00831-7.
[16]. Chandra Pal, A., Panda, M., and Bhuyan, P.K., A comprehensive study on sustainable development of pavement quality concrete utilising fly-ash and copper slag. European Journal of Environmental and Civil Engineering, 2025. 29(9): p. 1743-1768.DOI: 10.1080/19648189.2025.2453016.
[17]. Shirdam, R., Amini, M., and Bakhshi, N., Investigating the Effects of Copper Slag and Silica Fume on Durability, Strength, and Workability of Concrete. International Journal of Environmental Research, 2019. 13(6): p. 909-924.DOI: 10.1007/s41742-019-00215-7.
[18]. Sharmila, P. and Dhinakaran, G., Compressive strength, porosity and sorptivity of ultra fine slag based high strength concrete. Construction and Building Materials, 2016. 120: p. 48-53.DOI: 10.1016/j.conbuildmat.2016.05.090.
[19]. Zhou, Y., Sun, J., and Zhang, Z., Effects of High-Volume Ground Slag Powder on the Properties of High-Strength Concrete under Different Curing Conditions. Crystals, 2021. 11(4): p. 348.DOI: 10.3390/cryst11040348.
[20]. Xiao, H., et al., Graphene-iron ore tailings–based cementitious composites with high early flexural strength. 2022. 16(1): p. 327.
[21]. Wang, Y., et al., Utilization of waste phosphogypsum in high-strength geopolymer concrete: Performance optimization and mechanistic exploration. Journal of Building Engineering, 2024. 98: p. 111253.DOI: 10.1016/j.jobe.2024.111253.
[22]. Al-Oran, A.A.A., Safiee, N.A., and Nasir, N.A.M., Fresh and hardened properties of self-compacting concrete using metakaolin and GGBS as cement replacement. European Journal of Environmental and Civil Engineering, 2022. 26(1): p. 379-392.DOI: 10.1080/19648189.2019.1663268.
[23]. Lenka, B.P., Majhi, Rajib K., Singh, Subhralina, Nayak, Amar N., Eco-friendly and cost-effective concrete utilizing high-volume blast furnace slag and demolition waste with lime. European Journal of Environmental and Civil Engineering, 2022. 26(11): p. 5351-5373.DOI: 10.1080/19648189.2021.1896581.
[24]. Sathe, S. and Dandin, S., Experimental study of permeable concrete with FA and GGBS as partial replacement to cement. European Journal of Environmental and Civil Engineering, 2025. 29(5): p. 832-858.DOI: 10.1080/19648189.2024.2417674.
[25]. Kouider Djelloul, O., Menadi, B., and Kenai, S., The effect of slag and natural pozzolan on the rheological and compressive strength properties of recycled self-compacting mortar. European Journal of Environmental and Civil Engineering, 2024. 28(16): p. 3793-3810.DOI: 10.1080/19648189.2024.2357680.
[26]. Shirodkar, V., Patel, R., and Verma, M., Utilization of Red Mud in Cementitious Concrete-A Review. International Journal of Advanced Research in Engineering and Technology 2020. 11(2): p. 426-430.DOI: DOI:10.17605/OSF.IO/HGN3W.
[27]. Ribeiro, D.V., Labrincha, J.A., and Morelli, M.R., Effect of the addition of red mud on the corrosion parameters of reinforced concrete. Cement and Concrete Research, 2011. 42(1): p. 124-133.DOI: 10.1016/j.cemconres.2011.09.002.
[28]. Santos, L., Evaluation of the electrical resistivity of concrete as a parameter for the prediction of the initiation of corrosion induced by chlorides in concrete structures. 2006, MS thesis, University of Brasília, Brasília, DF.
[29]. Whiting, D.A. and Nagi, M.A., Electrical resistivity of concrete-a literature review. PCA R&D Serial, 2003. 2457: p. p. 426-430.DOI: DOI: 10.17605/OSF.IO/HGN3W.
[30]. Basheer, P.A.M., Gilleece, P. R. V., Long, A. E., Mc Carter, W. J., Monitoring electrical resistance of concretes containing alternative cementitious materials to assess their resistance to chloride penetration. Cement and Concrete Composites, 2002. 24(5): p. 437-449.DOI: 10.1016/s0958-9465(01)00075-0.
[31]. Azarsa, P. and Gupta, R., Electrical resistivity of concrete for durability evaluation: a review. Advances in Materials Science Engineering, 2017(1): p. 30.DOI: 10.1155/2017/8453095.
[32]. Spragg, R., Bu, Yiwen, Snyder, Kenneth, Bentz, Dale, Weiss, Jason., Electrical testing of cement-based materials: Role of testing techniques, sample conditioning, and accelerated curing. Joint Transportation Research Program, 2013.DOI: 10.5703/1288284315230.
[33]. Yuan, Q., Shi, C., De Schutter, G., Audenaert, K., Deng, D.,, Chloride binding of cement-based materials subjected to external chloride environment–a review. Construction and building materials, 2009. 23(1): p. 1-13.DOI: 10.1016/j.conbuildmat.2008.02.004.
[34]. Iran National Standards Organization (INSO), Portland cement-Specifications (In Persian), in INSO 389. 2020: Iran, .
[35]. British Standards Institution (BSI) BS EN 197-1: 2011 Cement-Part 1:, Composition, specifications and conformity criteria for common cements. 2011.DOI: 10.3403/30205527.
[36]. ASTMC150–07, Standard Test Method for Slump of Hydraulic-Cement Concrete, in ASTM International: West Conshohocken, PA, . 2012: USA, DOI: 10.1520/C0150-07.
[37]. ASTMC989/C989M-22, Standard Specification for Slag Cement for Use in Concrete and Mortars. DOI: 10.1520/C0989_C0989M-22, in ASTM International: West Conshohocken, PA, USA. 2022.
[38]. ASTMC494/C494M-13, Standard Specification for Chemical Admixtures for Concrete, in ASTM International: West Conshohocken, PA, . 2013: USA, . p. 10 DOI: 10.1520/C0494_C0494M-13.
[39]. ASTMC143/C143M–20, Standard Test Method for Slump of Hydraulic-Cement Concrete, in ASTM International: West Conshohocken, PA, DOI: 10.1520/C0143_C0143M-20. 2020: USA, .
[40]. ASTMC39/C39M-21, Standard Test Method for Compressive Strength of Cylindrical Concrete Specimens, in ASTM International: West Conshohocken, PA. 2023: USA, 10.1520/C0039_C0039M-21.
[41]. BS1881-122, Method for determination of water absorption, in British Standard Institution, . 2011, DOI: 10.3403/30242745.
[42]. NT Build 492, Chloride migration coefficient from non-steady state migration experiments. 1999: Nordtest, Finland, .
[43]. U.S. Environmental Protection Agency (USEPA), Method 1311: Toxicity Characteristics Leaching Procedure, SW-846: Test methods for evaluating solid waste, physical/chemical methods. 1998.
[44]. Snyder, K.A., Feng, X., Keen, BD., Mason, TO.,, Estimating the electrical conductivity of cement paste pore solutions from OH−, K+ and Na+ concentrations. Cement concrete research, 2003. 33(6): p. 793-798.DOI: 10.1016/S0008-8846(02)01068-2.
[45]. Hope, B., Nmai, C.K., ACI 222R-01, Protection of metals in concrete against corrosion. 2001, Technical Report for ACI Committee 222: Farmington Hills, MI: USA.
[46]. Teng, S., Lim, T.Y.D., and Sabet Divsholi, B., Durability and mechanical properties of high strength concrete incorporating ultra fine Ground Granulated Blast-furnace Slag. Construction and Building Materials, 2013. 40: p. 875-881.DOI: 10.1016/j.conbuildmat.2012.11.052.
[47]. U.S. Environmental Protection Agency (USEPA), Method 7000B: Test method for Flame Atomic Absorption Spectrophotometry. 2007, U. S. Environmental Protection Agency.
[48]. Shirdam, R., Nourigohar, A., and Mohamadi, S., Stabilization of filter cake and its leaching behaviour: a case study with cementitious and soluble phosphate additives. Pollution, 2019(3).DOI: 10.22059/poll.2019.274149.567.
[49]. Mahin Sha, O.B., Remya, C. P., Salja, P. A., Shifal, K. S., Red Mud Concrete. International Research Journal of Engineering and Technology, 2022. 3(4): p. 2582-2585.
[50]. Syam Sai, P., Sukesh, C.,, Strength properties of concrete by using red mud as a replacement of cement with hydrated lime. International Journal of Civil Engineering Technology, 2017. 8(3): p. 38-49.
[51]. Megat Johari, M.A., Brooks, J. J., Kabir, S., Rivard, P., Influence of supplementary cementitious materials on engineering properties of high strength concrete. Construction and Building Materials, 2011. 25(5): p. 2639-2648.DOI: 10.1016/j.conbuildmat.2010.12.013.
[52]. Duran Atiş, C. and Bilim, C., Wet and dry cured compressive strength of concrete containing ground granulated blast-furnace slag. Building and Environment, 2007. 42(8): p. 3060-3065.DOI: 10.1016/j.buildenv.2006.07.027.
[53]. Gholampour, A. and Ozbakkaloglu, T., Performance of sustainable concretes containing very high volume Class-F fly ash and ground granulated blast furnace slag. Journal of Cleaner Production, 2017. 162: p. 1407-1417.DOI: 10.1016/j.jclepro.2017.06.087.
[54]. Miralami, S.M., Hajati Ziabari, S., and Esfahani, M.R., The Effect of GGBFS with Steel and Carbon Fibers on the Mechanical Properties and Durability of Concrete. AUT Journal of Civil Engineering, 2022. 6(2): p. 319-336.DOI: 10.22060/ajce.2023.21616.5806.
[55]. Yazıcı, H., Yardımcı, M.Y., Yiğiter, H., Aydın, S. and Türkel, S., Mechanical properties of reactive powder concrete containing high volumes of ground granulated blast furnace slag. Cement Concrete Composites, 2010. 32(8): p. 639-648.DOI: 10.1016/j.cemconcomp.2010.07.005.
[56]. Oner, A., Akyuz, S., An experimental study on optimum usage of GGBS for the compressive strength of concrete. Cement and Concrete Composites, 2007. 29(6): p. 505-514.DOI: 10.1016/j.cemconcomp.2007.01.001.
[57]. Gruyaert, E., Robeyst, N., De, Belie N. and calorimetry, Study of the hydration of Portland cement blended with blast-furnace slag by calorimetry and thermogravimetry. Journal of thermal analysis, 2010. 102(3): p. 941-951.DOI: 10.1016/j.cemconcomp.2007.01.001.
[58]. Kocaba, V., Gallucci, E., Scrivener, K. L., Methods for determination of degree of reaction of slag in blended cement pastes. Cement Concrete Research, 2012. 42(3): p. 511-525.DOI: 10.1016/j.cemconres.2011.11.010.
[59]. Whittaker, M., Zajac, M., Haha, M. B., Bullerjahn, F., Black, L., The role of the alumina content of slag, plus the presence of additional sulfate on the hydration and microstructure of Portland cement-slag blends. Cement Concrete Research, 2014. 66: p. 91-101.DOI: 10.1016/j.cemconres.2014.07.018.
[60]. Lee, H.S., Wang, XY., Zhang, LN., Koh, KT., Analysis of the optimum usage of slag for the compressive strength of concrete. Materials (Bazel), 2015. 8(3): p. 1213–1229.DOI: 10.3390/ma8031213.
[61]. Rathod, H.A., and Pitroda, J.,, From Bricks To Blocks: A Masonary Unit From Western Gujarat Region Of India. International Journal of Engineering Trends Technology, 2013.DOI: 10.14445/22315381/IJETT-V4I6P123.
[62]. Shinge, K.S. and Pendhari, S.S., Use of Red Mud for Partial Cement Replacement. International Journal of Modern Trends in Engineering and Research, 2015.
[63]. Sowmyashree T., M.C.S., Arpitha D. J., Panditharadhya B. J. , Comparison on durability properties of red mud as a partial replacement of cement with hydrated lime for different grades of concrete with and without superplaticiser. Internationaljournal of Engineering Research and Technology, 2016. 5(5): p. 572-577.DOI: 10.17577/IJERTV5IS050856.
[64]. Nikbin, I.M., Aliaghazadeh, M., Sh, C., Fathollahpour, A., Environmental impacts and mechanical properties of lightweight concrete containing bauxite residue (red mud). Journal of Cleaner Production, 2018. 172: p. 2683-2694.DOI: 10.1016/j.jclepro.2017.11.143.
[65]. Luo, S., Liu, M., Yang, L., Chang, J., Yang, W., Yan, X., Yu, H., Shen, Y., Utilization of waste from alumina industry to produce sustainable cement-based materials. Construction and Building Materials, 2019. 229: p. 2683-2694.DOI: 10.1016/j.conbuildmat.2019.116795.
[66]. Dodoo-Arhin, D., Nuamah, R. A., Agyei-Tuffour, B., Obada, D. O., Yaya, A., Awaso bauxite red mud-cement based composites: Characterisation for pavement applications. Case Studies in Construction Materials, 2017. 7: p. 45-55.DOI: 10.1016/j.cscm.2017.05.003.
[67]. Tang, W.C., Wang, Z., Donne, S. W., Forghani, M. and Liu, Y., Influence of red mud on mechanical and durability performance of self-compacting concrete. J Hazard Mater, 2019. 379: p. 120802.DOI: 10.1016/j.jhazmat.2019.120802.
[68]. Ghalehnovi, M., et al., Effect of red mud (bauxite residue) as cement replacement on the properties of self-compacting concrete incorporating various fillers. Journal of Cleaner Production, 2019. 240: p. 118213.DOI: 10.1016/j.jclepro.2019.118213.
[69]. Venkatesh, C., Nerella, R., and Chand, M.S.R., Role of red mud as a cementing material in concrete: a comprehensive study on durability behavior. Innovative Infrastructure Solutions, 2020. 6(1): p. 13.DOI: 10.1007/s41062-020-00371-2.
[70]. ACI 363R-2001. American Concrete Institute Committee 363., Report on high-strength concrete. Farmington Hills (MI): American Concrete Institute; 2010. 65 p. ISBN: 9780870314612. .
[71]. ACI 363R-2005. American Concrete Institute Committee 363., High-strength concrete: ACI 363R [Internet]. Farmington Hills (MI):. American Concrete Institute; 2005.
[72]. ACI 363R-2010. American Concrete Institute Committee 363., Report on high-strength concrete: ACI 363R-10 [Internet]. Farmington Hills (MI):. American Concrete Institute; 2010
[73]. ACI-ASCE 441-96. Joint ACI-ASCE Committee 441., High strength concrete columns: ACI PRC-441-96. Farmington Hills (MI):. American Concrete Institute; 1996. 13 p. ISBN: 9780870314148.
[74]. ACI-ASCE 441, Report on equivalent rectangular concrete stress block and transverse reinforcement for high-strength concrete columns: ACI PRC-441.1-18. Farmington Hills (MI):. American Concrete Institute; 2018. 16 p. ISBN: 9781641950183., 2018.
[75]. Senff, L., Hotza, D., and Labrincha, J.A., Effect of red mud addition on the rheological behaviour and on hardened state characteristics of cement mortars. Construction and Building Materials, 2011. 25(1): p. 163-170.DOI: 10.1016/j.conbuildmat.2010.06.043.
[76]. Sabzi, J., Asadi Shamsabadi, E., Ghalehnovi, M., Hadigheh, S A., Khodabakhshian, A., Brito, J. d., Mechanical and durability properties of mortars incorporating red mud, ground granulated blast furnace slag, and electric arc furnace dust. Applied Sciences, 2021. 11(9): p. 4110.DOI: https://doi.org/10.3390/app11094110
[77]. Layssi, H., Ghods, P., Alizadeh, A. R., Salehi, M., Electrical resistivity of concrete. ACI Concrete international, 2015. 37(5): p. 41-46.DOI: 10.14359/51687832.
[78]. Andrade Perdrix, C., Calculation of chloride diffusion coefficients in concrete from ionic migration measurements. Cement and Concrete Research, 1993: p. 724-742.DOI: 10.1016/0008-8846(93)90023-3
[79]. Liu, Z., Zhang, Y., and Jiang, Q., Continuous tracking of the relationship between resistivity and pore structure of cement pastes. Construction and Building Materials, 2014. 53: p. 26-31.DOI: 10.1016/j.conbuildmat.2013.11.067.
[80]. Shi, C., Effect of mixing proportions of concrete on its electrical conductivity and the rapid chloride permeability test (ASTM C1202 or ASSHTO T277) results. Cement and Concrete Research, 2004. 34(3): p. 537-545.DOI: 10.1016/j.cemconres.2003.09.007.
[81]. Rajabipour, F. and Weiss, J., Electrical conductivity of drying cement paste. Materials and Structures, 2006. 40(10): p. 1143-1160.DOI: 10.1617/s11527-006-9211-z.
[82]. Bentz, D.P., A virtual rapid chloride permeability test. Cement Concrete Composites, 2007. 29(10): p. 723-731.DOI: 10.1016/j.cemconcomp.2007.06.006.
[83]. Angst, U.M., Geiker, M. R., Michel, A., Gehlen, C., Wong, H., Isgor, O. B., Elsener, B., Hansson, C. M., François, R., Hornbostel, K. , The steel–concrete interface. Materials Structures, 2017. 50(2): p. 143.DOI: 10.1617/s11527-017-1010-1.
[84]. Aı̈tcin, P.C., The durability characteristics of high performance concrete: a review. Cement and Concrete Composites, 2003. 25(4-5): p. 409-420.DOI: 10.1016/s0958-9465(02)00081-1.
[85]. Ortega, J.M., et al., Effects of Red Mud Addition in the Microstructure, Durability and Mechanical Performance of Cement Mortars. Applied Sciences, 2019. 9(5): p. 984.DOI: 10.3390/app9050984.
[86]. Florea, M.V.A., Brouwers, H.J.H., Chloride binding related to hydration products: Part I: Ordinary Portland Cement. Cement Concrete Research, 2012. 42(2): p. 282-290.DOI: 10.1016/j.cemconres.2011.09.016.
[87]. De Weerdt, K., Orsáková, D., Geiker, M.R., The impact of sulphate and magnesium on chloride binding in Portland cement paste. Cement Concrete Research, 2014. 65: p. 30-40.DOI: 10.1016/j.cemconres.2014.07.007.
[88]. Ogirigbo, O.R., Black, L., Chloride binding and diffusion in slag blends: Influence of slag composition and temperature. Construction and Building Materials, 2017. 149: p. 816-825.DOI: 10.1016/j.conbuildmat.2017.05.184.
[89]. Pontikes, Y. and Angelopoulos, G.N., Bauxite residue in cement and cementitious applications: Current status and a possible way forward. Resources, Conservation and Recycling, 2013. 73: p. 53-63.DOI: 10.1016/j.resconrec.2013.01.005.
[90]. Çelik, S., An experimental investigation of utilizing waste Red Mud in soil grouting. KSCE Journal of Civil Engineering, 2017. 21(4): p. 1191-1200.DOI: 10.1007/s12205-016-0774-0.
[91]. U.S. Environmental Protection Agency (USEPA), Introduction of hazardous waste identification, in (40CFR parts 261) EPA530-K-05-012, Washington, DC, USA: USEPA. 2005.
[92]. Council of the European Union, Council D., 33/EC of 19 December 2002 establishing criteria and procedures for the acceptance of waste at landfills pursuant to Article 16 of and Annex II to Directive 1999/31/EC. 2003.
[93]. EN12457-4: 2002. European Committee for Standardization., Characterization of waste: leaching; compliance test for leaching of granular waste materials and sludges. Part 4: one-stage batch test at a liquid-to-solid ratio of 10 L/kg for materials with particle size below 10 mm, without or with size reduction. . Brussels: CEN, 2002.
[94]. Özbay, E., Erdemir, M., and Durmuş, H.İ., Utilization and efficiency of ground granulated blast furnace slag on concrete properties – A review. Construction and Building Materials, 2016. 105: p. 423-434.DOI: 10.1016/j.conbuildmat.2015.12.153.
[95]. Gu, H., Tang, M., Wu, S., Wang, H., Meng, Z., Performance of cementitious composites with bayer red mud as a partial cement replacement. Sci Rep, 2025. 15(1): p. 44628.DOI: 10.1038/s41598-025-29623-w.

Articles in Press, Accepted Manuscript
Available Online from 22 November 2026